Photoresist Coating on Flexible Substrates: Ultrasonic Spray Deposition for PI and PET Films
Flexible electronics, flexible circuits, wearable sensors, and thin-film devices often use polymer substrates that cannot be processed like rigid silicon wafers. Polyimide (PI), polyethylene terephthalate (PET), and related films introduce challenges in wetting, dimensional stability, solvent compatibility, and handling. Photoresist coating on flexible substrates may benefit from ultrasonic spray deposition because the process is non-contact and can be configured for sheet-fed or continuous web workflows. This technical guide covers substrate preparation, spray parameters, drying, and process qualification for polymer films.
Flexible films require a different coating strategy
Rigid wafers are supported by a chuck and can often be rotated at high speed. Thin polymer films may wrinkle, stretch, flutter, or shift when subjected to similar handling. Their surfaces can have low surface energy, additives, protective liners, or prior treatments that change wetting. A coating method must account for the film’s mechanical behaviour as well as the chemistry of the photoresist.
PI and PET should not be treated as interchangeable. Polyimide is selected for applications that need higher temperature tolerance and dimensional stability, while PET may be used where optical clarity, flexibility, or cost is important. Specific grades, thicknesses, surface treatments, and coatings vary. Confirm solvent resistance and thermal limits using the actual film grade and supplier data before running a process trial.
Why consider ultrasonic photoresist coating
An ultrasonic nozzle uses high-frequency vibration to atomize liquid into droplets that are directed toward the substrate. A controlled spray path creates overlapping deposition tracks without requiring the film to rotate. The substrate can be supported on a flat carrier for sheet processing or transported through a coating station in a roll-to-roll arrangement. This non-contact approach can be useful where direct contact or high rotational forces are undesirable.
Uniformity still depends on the full process. Flow rate, atomization setting, nozzle distance, spray angle, carrier gas, traverse speed, track overlap, and web speed influence the deposited wet film. Resist viscosity, solids content, and solvent volatility influence droplet coalescence and drying. A process recipe should be developed on the same film grade, thickness, surface treatment, and handling configuration intended for production.
Surface energy, cleaning, and adhesion
Polymer films may arrive with corona treatment, plasma activation, primer layers, or protective coatings. Their surface energy can change during storage and handling. If a resist beads or retracts, first examine the substrate condition and cleaning history rather than immediately increasing the spray flow. Fingerprints, release-agent residues, dust, and roll-handling contamination can all affect wetting and adhesion.
Cleaning and activation methods must be compatible with the polymer and existing functional layers. Aggressive solvents can swell or craze some films, while excessive plasma treatment may alter the surface or reduce performance in later operations. Use a controlled preparation procedure and record the time between activation and coating. Adhesion should be evaluated after soft bake and again after development or the downstream etch process.
Sheet coating and web transport
For sheet processing, the film should be held flat without stretching or creating marks in the active region. Vacuum support or a carrier plate may be considered if compatible with the substrate and process. For roll-to-roll coating, stable web tension, lateral guiding, backing support, and speed control become essential. Web flutter changes the nozzle gap, while tension variation can change film dimensions and pattern registration.
Assess uniformity in both directions: across the web width and along the machine direction. A centre coupon alone cannot reveal edge thinning, nozzle banding, or drift during a long run. Sample the leading, middle, and trailing portions of the web and compare both edges with the centre. For multi-nozzle systems, match individual spray footprints and evaluate overlap zones to avoid longitudinal stripes.
Drying and polymer thermal budget
Solvent evaporation must be sufficient for the resist to become stable, but the drying process must remain within the polymer’s thermal limits. PI and PET can respond differently to temperature, tension, and solvent exposure. Excessive heat may cause shrinkage or dimensional change, while insufficient drying can leave residual solvent that affects winding, handling, adhesion, or exposure. The bake profile should be developed for the actual resist and film construction.
Inspect the film after drying for tack, curl, cracking, blocking, haze, and dimensional change. If the substrate is part of a multilayer stack, check whether the resist solvent affects adhesives, conductors, barrier layers, or prior coatings. Measure the final dry-film thickness and compare it with the wet-process settings. The goal is a repeatable dry film that supports lithography, not simply a visually continuous wet layer.
Lithography and mechanical reliability testing
Run the complete exposure and development sequence on representative coated films. Evaluate critical dimensions, adhesion, residue, and the ability of the resist to protect the substrate during the intended etch, plating, or lift-off process. Flexible devices may be bent or handled after patterning, so check whether the patterned resist or remaining stack cracks, delaminates, or changes dimension under the expected mechanical conditions.
Define test conditions that reflect the product rather than using arbitrary bend cycles or temperatures. Keep uncoated controls and record film lot, resist batch, surface treatment, bake history, and coating settings. If the process includes winding, evaluate the film after winding and unwinding to detect blocking or transfer. A successful flat coupon test is only the first stage of qualification.
Scale-up and process control
Before production release, repeat the recipe across multiple film lots and after routine nozzle cleaning. Monitor flow stability, web speed, tension, nozzle condition, environmental conditions, and drying performance. Set limits for thickness variation, defect density, edge quality, and dimensional change. Establish inspection points that can detect drift before a full roll or batch is affected.
Equipment selection should include substrate width, supported film thickness, fixture design, motion axes, web handling, enclosure, exhaust, solvent compatibility, recipe storage, and cleaning access. Production teams should review changeover time and the method for purging or replacing resist. A documented operating window helps transfer the process between operators and shifts.
For PI and PET, the trial plan should also include the mechanical condition of the film before and after coating. Measure dimensional change in both the machine and transverse directions where applicable, and inspect for curl, wrinkles, edge damage, and blocking after drying or winding. If a flexible device will be bent after patterning, evaluate the relevant stack under the intended bend radius and handling sequence rather than relying on a generic flexibility claim. Include at least one test at the expected production speed because a slow laboratory pass may allow more drying time than the production line. These checks connect the coating recipe to the actual converting process and help reveal limitations before scale-up.
Conclusion and contact
Ultrasonic spray deposition is a candidate approach for photoresist coating on flexible substrates such as PI and PET when non-contact handling and adaptable coverage are important. Its performance depends on substrate surface condition, web stability, resist compatibility, drying, and downstream lithography. Use representative films and the complete device process to qualify the coating window.
See [ultrasonic coating equipment solutions](https://cheersonic-liquid.com/en/ultrasonic-coating-equipment-solutions/) and [photoresist deposition for microelectronics](https://cheersonic-liquid.com/en/photoresist-deposition-for-microelectronics/). Flexible-electronics manufacturers and R&D teams can email market2@cheersonic.com to discuss a coating project and arrange a sample test on their PI, PET, or other flexible substrates.