Ultrathin and Uniform Insulation Coatings: Ultrasonic Spray Coating for Busbar Insulation Protection — From Dielectric Ink Composition Analysis to Process Scale-Up
Abstract
With the rapid development of electric vehicles, energy storage converters, photovoltaic inverters, and silicon carbide (SiC) high-frequency power electronics, electrical busbar insulation systems are facing increasingly demanding requirements for electrical reliability, thermal stability, power density, and compact structural integration.
Conventional electrostatic powder coating, dip coating, and film lamination technologies present certain limitations in complex geometry coverage, ultrathin coating fabrication, localized thickness control, and functional material deposition. Developing insulation coating technologies capable of precise liquid delivery, controlled atomization, and uniform material deposition is therefore of considerable importance for advanced busbar manufacturing.
This study proposes an ultrasonic spray coating (USC) methodology for manufacturing electrical insulation and protective coatings on busbar substrates. Liquid epoxy resin is selected as the insulating polymer matrix, while nanoscale aluminum oxide (Al2O3) is introduced as the functional filler.
By adjusting the insulating matrix-to-nanoparticle mass ratio (I-NP) and the solvent-to-nanoparticle mass ratio (S-NP), the proposed experimental program systematically investigates the influence of dielectric ink composition on dispersion stability, rheological properties, ultrasonic atomization behavior, coating morphology, and electrical insulation performance.
A quantitative relationship between liquid flow rate, nozzle scanning speed, scanning path spacing, deposition passes, and dry-film thickness is subsequently established. The influence of deposition parameters on coating thickness uniformity, surface roughness, pinhole formation, interfacial adhesion, and partial discharge characteristics is examined.
Optical microscopy, scanning electron microscopy (SEM), surface profilometry, insulation resistance measurements, dielectric breakdown testing, Partial Discharge Inception Voltage (PDIV) measurements, and environmental reliability testing are incorporated into a comprehensive evaluation framework.
Finally, the proposed ultrasonic spray coating process is scaled from small-area copper specimens to 100 cm2 copper substrates to investigate changes in coating uniformity, material delivery stability, scanning strategies, and electrical reliability during process scale-up.
The objective of this research is to establish relationships among dielectric ink formulation, ultrasonic atomization and deposition parameters, coating microstructure, and electrical insulation properties, providing an experimental framework for manufacturing ultrathin and highly uniform busbar insulation coatings.
Keywords: Busbar; Busbar Insulation Coating; Ultrasonic Spray Coating; Dielectric Ink; Nano-Alumina; Ultrathin Insulation Coating; Partial Discharge Inception Voltage; PDIV; Coating Uniformity; Process Scale-Up.
1. Introduction
The rapid development of electric vehicles, battery energy storage systems, photovoltaic power generation, and wide-bandgap semiconductor technologies is driving electrical interconnection systems toward higher operating voltages, higher currents, faster switching frequencies, and greater power density.
As essential electrical interconnection components between power modules, capacitors, battery systems, and power conversion equipment, busbars directly influence the electrical performance, thermal behavior, and operational reliability of modern power electronic systems.
In particular, busbars used in 800 V-class electric vehicle drive systems, 1,500 V-class energy storage converters, and SiC-based high-frequency inverters must withstand not only continuous electrical stress but also rapid voltage transitions, localized electric field concentration, thermal cycling, and long-term environmental degradation.
Conventional busbar insulation technologies include polyimide film lamination, epoxy powder coating, fluidized bed coating, liquid dielectric varnish dip coating, and resin encapsulation.
Epoxy powder coating offers favorable mechanical properties, established manufacturing processes, and large-scale production capabilities. However, certain limitations remain in precision thin-film thickness adjustment, localized coating deposition, and complex geometrical coverage.
Conventional pneumatic liquid spraying provides relatively broad material compatibility. Nevertheless, variations in droplet velocity, atomization behavior, spraying distance, and liquid flow may result in localized thickness fluctuations, overspray, and insufficient edge coverage.
For highly integrated busbars, excessive insulation thickness may affect installation space, thermal resistance, component assembly, and electrical connection tolerances.
Therefore, developing thinner, more uniform, and more controllable insulation coatings while maintaining sufficient electrical reliability represents an important research direction in advanced busbar manufacturing.
Ultrasonic spray coating utilizes high-frequency mechanical vibrations to atomize liquid formulations into fine droplets. These droplets are transported toward the substrate using controlled shaping airflow and deposited through programmable motion systems.
Compared with conventional high-pressure pneumatic spraying, ultrasonic spray coating offers potential advantages under suitable material and processing conditions:
- Precise liquid flow rate control.
- Stable atomization at relatively low flow rates.
- Programmable material deposition trajectories.
- Multiple thin-film deposition passes.
- Localized functional coating.
- Potential improvement in material utilization.
- Compatibility with automated and flexible manufacturing.
- Compatibility with selected micro- and nanoparticle-containing functional inks.
However, the final coating quality depends not only on ultrasonic atomization equipment but also on dielectric ink viscosity, surface tension, solids content, filler particle size, solvent evaporation behavior, and substrate wettability.
For nanocomposite dielectric inks, insufficient filler loading may limit functional material modification. Excessive filler loading may increase particle agglomeration, ink viscosity, liquid delivery instability, and coating porosity.
A systematic investigation of dielectric ink formulation, ultrasonic atomization, droplet deposition, film formation, and electrical insulation performance is therefore necessary.
The proposed research consists of three major experimental stages.
Stage 1: Dielectric Ink Formulation Screening
The insulating matrix-to-nanoparticle mass ratio and solvent-to-nanoparticle mass ratio are adjusted to investigate dispersion stability, sprayability, film formation, and electrical insulation properties.
Stage 2: Deposition Process Optimization
Liquid flow rate, nozzle scanning speed, scanning path spacing, and deposition passes are investigated to establish relationships among coating thickness, surface morphology, material utilization, and deposition efficiency.
Stage 3: Scale-Up to 100 cm2 Coating Area
The coating process developed using small-area copper specimens is extended to larger substrates.
The influence of process scale-up on thickness uniformity, edge effects, continuous operating stability, and electrical performance consistency is evaluated.
Through these investigations, the applicability of ultrasonic precision spray coating to busbar insulation manufacturing can be systematically assessed, providing a foundation for subsequent development of three-dimensional busbar coating processes and automated production lines.
2. Experimental Section
2.1 Preparation of Insulation Coatings by Ultrasonic Spray Coating
The proposed experimental methodology employs liquid epoxy-based dielectric inks to prepare nanocomposite insulation coatings on copper substrates using ultrasonic precision spray coating equipment.
The principal experimental materials and their respective functions are summarized in Table 1.
Table 1. Experimental Materials and Their Functions
| Experimental Material | Primary Function |
|---|---|
| Liquid Epoxy Resin | Formation of the continuous insulating polymer matrix |
| Compatible Curing Agent | Promotion of polymer crosslinking |
| Nano-Al2O3 | Modification of dielectric properties and coating microstructure |
| Nano-SiO2 | Optional interfacial and dielectric modification |
| Boron Nitride (BN) | Optional thermally conductive insulation filler |
| Silane Coupling Agent | Improvement of filler-to-polymer compatibility |
| Compatible Solvent | Adjustment of ink viscosity and atomization behavior |
| Dispersant | Improvement of nanoparticle dispersion stability |
| Defoaming Agent | Reduction of entrapped air and bubbles |
| Copper Plates and Busbars | Substrates for dielectric coating deposition |
During the initial experimental stage, nano-Al2O3 is selected as the primary functional filler to minimize variables associated with multiple-filler systems.
Following establishment of stable dielectric ink formulations and coating processes, further investigations may incorporate BN/Al2O3 or SiO2/Al2O3 hybrid filler systems.
2.1.1 Preparation of Samples for Dielectric Ink Formulation Screening
(1) Dielectric Ink Composition Design
The dielectric ink primarily consists of an insulating polymer matrix, nanoparticles, solvents, and functional additives.
Two principal formulation variables are introduced to investigate the effects of material composition on ultrasonic spraying and electrical insulation performance.
The insulating matrix-to-nanoparticle mass ratio is defined as:
I-NP = M_matrix / M_NP
Where:
- M_matrix is the total nonvolatile mass of the insulating resin and curing agent.
- M_NP is the mass of the nanoparticle filler.
The solvent-to-nanoparticle mass ratio is defined as:
S-NP = M_solvent / M_NP
Where:
- M_solvent is the total solvent mass in the dielectric ink.
- M_NP is the nanoparticle filler mass.
Both parameters are expressed as mass ratios.
The I-NP ratio is used to investigate the relationship between the continuous insulating polymer phase and functional nanoparticle loading.
The S-NP ratio is used to investigate ink dilution, rheological properties, ultrasonic atomization stability, droplet spreading, and film formation.
(2) Experimental Design for I-NP Ratio Screening
Five nanoparticle-containing dielectric ink formulations and one unfilled epoxy reference formulation are proposed.
Table 2. I-NP Ratio Screening Formulations
| Sample ID | Insulating Matrix Mass | Nano-Al2O3 Mass | I-NP Ratio | Filler Content in Dry Film |
|---|---|---|---|---|
| I-0 | 10.0 g | 0 g | Reference | 0% |
| I-1 | 9.5 g | 0.5 g | 19:1 | 5% |
| I-2 | 9.0 g | 1.0 g | 9:1 | 10% |
| I-3 | 8.5 g | 1.5 g | 5.67:1 | 15% |
| I-4 | 8.0 g | 2.0 g | 4:1 | 20% |
| I-5 | 7.5 g | 2.5 g | 3:1 | 25% |
The calculations presented above exclude small quantities of nonvolatile functional additives.
The resin-to-curing-agent ratio must remain consistent with the stoichiometric requirements of the selected epoxy system.
Changes in nanoparticle loading should not alter the required resin-to-curing-agent ratio.
To minimize the influence of solvent concentration during I-NP ratio screening, the total theoretical mass solids content of each formulation may initially be maintained at 20%.
For each formulation, approximately 40 g of compatible solvent is added to 10 g of nonvolatile primary materials to produce 50 g of dielectric ink.
If the selected resin already contains solvent or additional nonvolatile additives are incorporated, the actual solids content must be recalculated.
This experimental approach enables comparison of the influence of nanoparticle loading on rheological behavior, coating morphology, and electrical insulation properties under approximately equivalent mass solids content.
(3) Experimental Design for S-NP Dilution Ratio Screening
Following preliminary I-NP ratio screening, a formulation exhibiting suitable sprayability and electrical insulation properties should be selected for further investigation of solvent concentration.
An I-NP ratio of 9:1 is used in the following illustrative experimental design.
This ratio is not presented as an experimentally established optimum.
Table 3. S-NP Dilution Ratio Screening Formulations
| Sample ID | Insulating Matrix | Nano-Al2O3 | Solvent Mass | S-NP Ratio | Theoretical Mass Solids Content |
|---|---|---|---|---|---|
| S-1 | 9 g | 1 g | 15.00 g | 15:1 | 40% |
| S-2 | 9 g | 1 g | 23.33 g | 23.33:1 | 30% |
| S-3 | 9 g | 1 g | 40.00 g | 40:1 | 20% |
| S-4 | 9 g | 1 g | 56.67 g | 56.67:1 | 15% |
| S-5 | 9 g | 1 g | 90.00 g | 90:1 | 10% |
These formulations cover a range of relatively high-solids and low-solids dielectric ink systems.
The objective is to investigate how solvent dilution influences ultrasonic atomization stability, material deposition efficiency, droplet spreading, and final coating quality.
If a formulation exceeds the allowable viscosity or liquid delivery capacity of the selected ultrasonic nozzle, the incompatibility should be documented rather than forcing the coating process beyond validated equipment limits.
(4) Nanoparticle Dispersion and Dielectric Ink Preparation
Nano-Al2O3 particles exhibit a relatively high specific surface area and may form agglomerated structures through interparticle interactions.
The dielectric ink preparation process must therefore emphasize nanoparticle dispersion and filler-to-polymer compatibility.
The proposed preparation workflow is:
Nanoparticle Pretreatment → Solvent Predispersion → Addition of Dispersants or Coupling Agents → Mechanical Mixing → Ultrasonic Dispersion → Epoxy Resin Incorporation → Curing Agent Addition → Degassing → Compatible Filtration → Precision Liquid Delivery.
Initially, nanoparticles should be dried or surface-treated according to supplier recommendations to reduce the influence of adsorbed moisture.
The nanoparticles are subsequently introduced into a portion of the selected solvent and subjected to mechanical mixing and ultrasonic dispersion to reduce agglomeration.
The resulting nanoparticle suspension is incorporated into the epoxy resin system.
After sufficient mixing, the compatible curing agent is added according to the specified resin-to-curing-agent ratio.
During preparation, the following parameters should be recorded:
- Ink temperature.
- Mechanical mixing duration.
- Ultrasonic dispersion duration.
- Ink viscosity.
- Dispersion stability.
- Storage duration.
- Formulation pot life.
Appropriate degassing and filtration procedures are subsequently used to remove entrapped air and abnormal oversized particles.
For nanoparticle-containing dielectric inks, filtration should not remove a significant proportion of the intended functional fillers.
Excessive filler removal may alter the original I-NP ratio and compromise formulation consistency.
The prepared dielectric ink should be sprayed within its validated processing and storage stability window.
(5) Copper Substrate Pretreatment
Copper plates measuring 50 mm x 50 mm are proposed for the initial experimental stage.
The nominal single-side coating area is 25 cm2.
A substrate thickness of approximately 1 mm may be selected as an experimental reference.
Copper substrates should preferably be obtained from the same material batch to minimize variations in surface composition and material properties.
The proposed substrate pretreatment workflow is:
Surface Inspection → Degreasing → Compatible Surface Treatment → Rinsing → Drying → Surface Cleanliness Verification → Ultrasonic Spray Coating.
Copper surface roughness and cleanliness should remain reasonably consistent throughout the experimental program.
Subsequent investigations may compare controlled mechanical roughening, chemical conversion treatment, and plasma surface activation to evaluate their effects on coating adhesion and long-term electrical reliability.
(6) Ultrasonic Spray Coating Experimental Equipment
The proposed ultrasonic spray coating system consists of the following components:
- Ultrasonic atomizing nozzle.
- Ultrasonic generator.
- Precision liquid metering pump.
- Automated XYZ motion platform.
- Controlled shaping airflow system.
- Temperature-controlled substrate stage.
- Workpiece positioning fixtures.
- Ink storage and circulation system.
- Programmable coating control software.
- Ventilation and appropriate safety protection systems.
The dielectric ink is delivered to the ultrasonic nozzle through a precision metering pump.
High-frequency mechanical vibrations generate fine droplets at the atomizing surface.
The droplets are directed toward the copper substrate through a controlled airflow system and deposited according to predefined scanning trajectories.
A 60 kHz ultrasonic nozzle may be selected as an initial experimental configuration.
However, the operating frequency, atomization power, flow rate capacity, and nozzle geometry must be determined according to actual equipment specifications and dielectric ink properties.
Table 4. Suggested Initial Ultrasonic Spray Coating Parameters
| Process Parameter | Suggested Initial Condition |
|---|---|
| Ultrasonic Nozzle Frequency | 60 kHz, equipment dependent |
| Liquid Flow Rate | 0.3 mL/min |
| Scanning Speed | 50 mm/s |
| Scanning Path Spacing | 3 mm |
| Nozzle-to-Substrate Distance | 50 mm |
| Substrate Temperature | 40-60°C |
| Coating Trajectory | Parallel raster scanning |
| Number of Deposition Passes | Determined by target dry-film thickness |
| Intermediate Drying | Validated for the selected solvent system |
| Final Curing | According to the epoxy resin curing specification |
These parameters are proposed starting conditions for process development.
They do not represent experimentally verified equipment capabilities or optimized manufacturing conditions.
For dielectric inks containing flammable solvents, spraying equipment, heating systems, ventilation, and electrical installations must comply with applicable fire protection, explosion prevention, and occupational safety requirements.
(7) Drying and Curing
Following ultrasonic spray coating, the deposited dielectric films should undergo controlled drying and final curing according to the selected epoxy system.
The initial drying stage primarily facilitates solvent evaporation and reduces the risk of residual solvent entrapment and bubble formation.
The subsequent curing stage promotes polymer crosslinking and formation of the final insulating coating structure.
Where necessary, post-curing may be introduced to improve the degree of crosslinking and thermal stability.
Curing temperatures, heating rates, and holding times must be determined according to resin supplier recommendations, DSC measurements, and experimental film formation results.
Comparable and compatible curing conditions should be maintained across different formulations to support meaningful experimental comparisons.
2.1.2 Investigation of Liquid Flow Rate and Scanning Speed
Following dielectric ink formulation screening, a suitable formulation should be selected for systematic investigation of deposition process parameters.
Liquid flow rate determines the quantity of coating material delivered to the ultrasonic nozzle per unit time.
Scanning speed determines the residence time of the spray pattern over a given substrate region.
Together, these parameters influence:
- Material deposition per unit area.
- Wet-film thickness.
- Droplet overlap.
- Solvent evaporation.
- Dry-film thickness.
- Coating uniformity.
- Manufacturing throughput.
(1) Liquid Flow Rate Investigation
The following liquid flow rate levels are proposed.
Table 5. Liquid Flow Rate Experimental Design
| Sample ID | Liquid Flow Rate | Scanning Speed | Path Spacing |
|---|---|---|---|
| F-1 | 0.1 mL/min | 50 mm/s | 3 mm |
| F-2 | 0.2 mL/min | 50 mm/s | 3 mm |
| F-3 | 0.3 mL/min | 50 mm/s | 3 mm |
| F-4 | 0.5 mL/min | 50 mm/s | 3 mm |
| F-5 | 0.8 mL/min | 50 mm/s | 3 mm |
| F-6 | 1.0 mL/min | 50 mm/s | 3 mm |
The objective is to investigate the influence of liquid flow rate under constant scanning conditions.
The primary evaluation parameters include:
- Atomization stability.
- Effective spray pattern width.
- Material deposition per unit area.
- Dry-film thickness.
- Surface roughness.
- Pinhole and bubble formation.
- Electrical insulation performance.
- Effective material transfer efficiency.
(2) Scanning Speed Investigation
Following preliminary confirmation of stable liquid delivery and atomization, different nozzle scanning speeds are investigated.
Table 6. Scanning Speed Experimental Design
| Sample ID | Liquid Flow Rate | Scanning Speed | Path Spacing |
|---|---|---|---|
| V-1 | 0.3 mL/min | 20 mm/s | 3 mm |
| V-2 | 0.3 mL/min | 35 mm/s | 3 mm |
| V-3 | 0.3 mL/min | 50 mm/s | 3 mm |
| V-4 | 0.3 mL/min | 75 mm/s | 3 mm |
| V-5 | 0.3 mL/min | 100 mm/s | 3 mm |
This experimental stage examines the influence of scanning speed on droplet overlap, material deposition, coating thickness, and surface uniformity.
(3) Combined Investigation of Liquid Flow Rate and Scanning Speed
A three-factor, three-level experimental design is proposed to investigate interactions among the principal deposition parameters.
Table 7. Process Parameter Optimization Levels
| Process Parameter | Low Level | Intermediate Level | High Level |
|---|---|---|---|
| Liquid Flow Rate | 0.2 mL/min | 0.5 mL/min | 0.8 mL/min |
| Scanning Speed | 25 mm/s | 50 mm/s | 100 mm/s |
| Path Spacing | 2 mm | 3 mm | 4 mm |
A full factorial experimental design consisting of 27 process combinations may be used.
Alternatively, an appropriately designed orthogonal experimental program may be employed when laboratory resources are limited.
A full factorial design provides opportunities to evaluate interactions among flow rate, scanning speed, and path spacing.
At least three independently prepared specimens are recommended for each initial process condition.
A larger number of independent specimens or valid independent test locations should be used for statistical dielectric breakdown evaluation.
(4) Theoretical Material Deposition Model
Under stable liquid flow rate, scanning speed, and path spacing conditions, the ideal wet-film thickness deposited during one complete raster scan can be estimated using the following equation:
D_wet = 1000 x Q / (60 x v x p)
Where:
- D_wet is the ideal average wet-film thickness in mm.
- Q is the liquid flow rate in mL/min.
- v is the scanning speed in mm/s.
- p is the spacing between adjacent scanning paths in mm.
Considering the volume solids fraction and effective material transfer efficiency, the theoretical average dry-film thickness can be estimated as:
T_dry = 1000000 x Q x phi x eta x N / (60 x v x p)
Where:
- T_dry is the theoretical average dry-film thickness in microns.
- Q is the liquid flow rate in mL/min.
- phi is the nonvolatile volume fraction of the dielectric ink.
- eta is the effective solids deposition efficiency.
- N is the number of complete area-scanning passes.
- v is the scanning speed in mm/s.
- p is the scanning path spacing in mm.
Both phi and eta must be entered as decimal fractions.
For example, a volume solids content of 15% should be entered as 0.15.
An effective deposition efficiency of 80% should be entered as 0.80.
Volume solids content and mass solids content are not equivalent.
The volume solids fraction should be calculated from material densities and nonvolatile contents or determined through appropriate experimental measurements.
This simplified model assumes approximately uniform steady-state deposition.
It does not explicitly account for droplet rebound, edge overspray, substrate wettability variations, acceleration and deceleration, or additional curing-related volume shrinkage.
(5) Illustrative Dry-Film Thickness Calculation
Assume the following coating conditions:
- Liquid flow rate: 0.3 mL/min.
- Scanning speed: 50 mm/s.
- Path spacing: 3 mm.
- Volume solids content: 15%.
- Effective deposition efficiency: 80%.
The theoretical average dry-film thickness for one complete area scan is:
T_dry = 1000000 x 0.3 x 0.15 x 0.80 / (60 x 50 x 3)
T_dry = 4 microns.
The estimated coating thicknesses for different numbers of deposition passes are summarized in Table 8.
Table 8. Theoretical Dry-Film Thickness for Multiple Deposition Passes
| Complete Area-Scanning Passes | Theoretical Average Dry-Film Thickness |
|---|---|
| 1 | 4 microns |
| 3 | 12 microns |
| 5 | 20 microns |
| 8 | 32 microns |
| 10 | 40 microns |
| 15 | 60 microns |
These values are theoretical calculations rather than experimental measurements.
Actual coating thickness should be measured using suitable surface profilometry, calibrated eddy-current thickness measurements, or cross-sectional microscopy.
A process-specific calibration relationship should subsequently be established between theoretical and measured deposition thickness.
The ultrathin coating thicknesses proposed in this study are intended for experimental investigation.
They must not be directly interpreted as validated safety insulation thicknesses for 800 V or 1,500 V busbar applications.
2.1.3 Preparation of 100 cm2 Scale-Up Specimens
Following dielectric ink formulation screening and preliminary process optimization, ultrasonic spray coating is extended to copper substrates with a nominal coating area of 100 cm2.
Copper plates measuring 100 mm x 100 mm are selected for the scale-up investigation.
Compared with the initial 25 cm2 specimens, the coating area is increased by a factor of four.
(1) Fundamental Principles of Process Scale-Up
The primary scale-up principle is to maintain approximately equivalent material deposition per unit area.
The following parameters should remain consistent wherever practical:
- Dielectric ink formulation.
- Ink solids content.
- Ultrasonic nozzle frequency.
- Liquid flow rate.
- Scanning speed.
- Scanning path spacing.
- Number of deposition passes.
- Nozzle-to-substrate distance.
- Substrate temperature.
- Final curing conditions.
The larger coating area is achieved by increasing scanning path length and the number of raster trajectories.
(2) Scanning Trajectory Design
Three different scanning strategies are proposed to investigate coating uniformity during area scale-up.
Strategy A: Unidirectional Raster Scanning
All deposition cycles use parallel raster scanning in the same principal orientation.
Strategy B: 90-Degree Crosshatch Scanning
Successive complete deposition cycles alternate between the X-direction and Y-direction.
Strategy C: Crosshatch Scanning with Edge Compensation
Additional localized coating passes are applied to designated edge regions following crosshatch scanning.
Table 9. Scanning Strategies for 100 cm2 Scale-Up Specimens
| Sample ID | Coating Area | Scanning Strategy | Edge Compensation |
|---|---|---|---|
| L-1 | 100 cm2 | Unidirectional raster scanning | No |
| L-2 | 100 cm2 | 90-degree crosshatch scanning | No |
| L-3 | 100 cm2 | 90-degree crosshatch scanning | Yes |
Actual coating material consumption, spraying duration, and average dry-film thickness should be recorded for all experimental groups.
For specimens incorporating localized edge reinforcement, material consumption associated with the primary coating and supplementary edge coating should be recorded separately.
(3) Material Consumption and Processing Time Estimation
At equivalent average dry-film thickness, the theoretical retained coating mass for a 100 cm2 specimen is approximately four times that of a 25 cm2 specimen.
Assume the following scale-up conditions:
- Coating area: 100 cm2, equivalent to 0.01 square meters.
- Target dry-film thickness: 30 microns.
- Cured coating density: 1.4 g/cm3.
- Ink mass solids content: 20%.
- Effective material transfer efficiency: 80%.
- Ink density: 1.0 g/mL.
- Liquid flow rate: 0.3 mL/min.
The theoretical dry coating mass is:
M_dry = 0.01 x 30 x 1.4
M_dry = 0.42 g.
The estimated liquid ink consumption is:
M_ink = 0.42 / (0.20 x 0.80)
M_ink = 2.625 g.
Assuming an ink density of 1.0 g/mL, the corresponding liquid volume is approximately 2.625 mL.
The theoretical effective liquid delivery time is:
T_delivery = 2.625 / 0.3
T_delivery = 8.75 minutes.
Actual manufacturing cycle time must additionally account for:
- Scanning direction changes.
- Nozzle start and stop operations.
- Acceleration and deceleration.
- Edge overspray.
- Intermediate drying.
- Workpiece handling.
- Final curing.
- Equipment positioning.
Consequently, process scale-up should evaluate not only coating quality but also material consumption, manufacturing throughput, and operational efficiency.
2.2 Morphological Characterization
Morphological characterization is performed to establish relationships between ultrasonic spray coating parameters and the resulting coating microstructure.
(1) Optical Microscopy
Optical microscopy is used to examine coating surfaces and edge regions.
The primary defects of interest include:
- Pinholes.
- Air bubbles.
- Particle agglomerates.
- Scanning patterns and coating streaks.
- Surface cracks.
- Exposed copper regions.
- Discontinuous edge coverage.
- Coating shrinkage.
- Sagging and localized accumulation.
Image analysis software may be used to quantify visible defect density and defective surface area.
Magnification and minimum detectable defect size should be recorded.
The absence of optically detectable defects does not establish the complete absence of microscopic coating defects.
(2) Scanning Electron Microscopy
Scanning Electron Microscopy (SEM) is used to investigate coating surface and cross-sectional morphology.
The primary characterization objectives include:
- Nanoparticle distribution.
- Particle agglomeration.
- Continuity of the polymer matrix.
- Internal coating porosity.
- Copper-to-coating interfacial structure.
- Local coating thickness.
- Interlayer structures formed through multiple deposition passes.
For different I-NP formulations, particular attention should be paid to the influence of nanoparticle loading on coating density, polymer continuity, and interfacial defects.
(3) Energy-Dispersive X-Ray Spectroscopy
Energy-Dispersive X-Ray Spectroscopy (EDS) is used to investigate the elemental distribution within selected coating cross-sections.
Elemental mapping of aluminum, oxygen, and other relevant elements can provide supporting information regarding Al2O3 filler distribution.
However, EDS spatial resolution depends on electron beam interaction volume and measurement conditions.
A relatively uniform elemental distribution does not necessarily establish that every nanoparticle is individually dispersed.
(4) Surface Roughness Measurement
Surface profilometry, three-dimensional optical microscopy, or Atomic Force Microscopy (AFM) may be used to characterize coating surface roughness.
Relevant parameters include:
- Ra: Arithmetic mean profile roughness.
- Rq: Root mean square profile roughness.
- Sa: Arithmetic mean surface height.
- Sq: Root mean square surface height.
Comparable evaluation lengths, scanning areas, and filtering conditions should be used across different experimental groups.
(5) Coating Thickness Measurement
Calibrated eddy-current thickness measurement may be used for nonconductive coatings deposited on conductive copper substrates.
Surface profilometry and cross-sectional microscopy should be used where necessary to validate thickness measurements.
For 25 cm2 specimens, a nine-point thickness measurement procedure is recommended.
For 100 cm2 scale-up specimens, at least 25 measurement locations are recommended.
For ultrathin coatings, instrument resolution, substrate compatibility, measurement uncertainty, and edge-related measurement errors must be evaluated before interpreting the results.
2.3 Electrical Performance and Reliability Characterization During Dielectric Ink Formulation Screening
2.3.1 Testing Equipment
A comprehensive material characterization platform should be established to evaluate the influence of I-NP and S-NP ratios on coating properties.
Table 10. Testing Equipment for Dielectric Ink Formulation Screening
| Testing Equipment | Primary Application |
|---|---|
| Rotational Viscometer or Rheometer | Ink viscosity and rheological properties |
| Surface Tension Measurement System | Dielectric ink surface tension |
| Contact Angle Measurement System | Wettability of copper substrates |
| Particle Size Analyzer | Particle or agglomerate size distribution |
| Precision Electronic Balance | Material mass and coating deposition |
| High-Resistance Meter | Insulation resistance and resistivity |
| High-Voltage Dielectric Strength Tester | Breakdown voltage and breakdown strength |
| Partial Discharge Measurement System | PDIV and discharge characteristics |
| Impedance Analyzer | Relative permittivity and dielectric loss |
| Temperature and Humidity Chamber | Damp-heat aging |
| Thermal Cycling Chamber | Thermal cycling reliability |
| Differential Scanning Calorimetry (DSC) | Curing behavior and glass transition |
| Thermogravimetric Analysis (TGA) | Thermal stability |
| Cross-Cut or Pull-Off Adhesion Equipment | Coating-to-substrate adhesion |
For electrical testing, the copper substrate may serve as the bottom electrode.
An appropriate upper electrode should be selected according to the applicable measurement procedure.
Guarded electrode configurations may be required for volume resistivity and dielectric measurements to minimize interference from surface leakage currents.
All high-voltage electrical tests must be performed in appropriately equipped laboratories with suitable electrical interlocks, protective barriers, discharge procedures, and grounding systems.
2.3.2 Testing Items
(1) Dielectric Ink Dispersion Stability
Ink appearance, viscosity, and sedimentation behavior should be recorded at defined intervals following formulation preparation.
Suggested observation intervals include:
- Initial condition.
- 30 minutes.
- 1 hour.
- 2 hours.
- 4 hours.
- Maximum validated formulation pot life.
For two-component epoxy formulations, nanoparticle sedimentation must be distinguished from viscosity changes associated with polymer curing reactions.
Where necessary, nanoparticle dispersion stability before curing agent addition should be evaluated separately from the processing stability of the fully formulated dielectric ink.
(2) Insulation Resistance and Volume Resistivity
Insulation resistance should be measured under defined voltage, environmental, and electrification-time conditions.
For an appropriate planar electrode configuration, volume resistivity can be calculated as:
rho_v = R x A / d
Where:
- rho_v is the volume resistivity.
- R is the measured volume resistance.
- A is the effective electrode area.
- d is the coating thickness.
A consistent unit system must be used.
For example, when resistance is expressed in ohms, electrode area in square meters, and thickness in meters, volume resistivity is expressed in ohm-meters.
(3) Dielectric Breakdown Strength
Dielectric breakdown voltage is measured using a defined electrode configuration and voltage application procedure.
The apparent dielectric breakdown strength can be calculated as:
E_b = U_b / d
Where:
- E_b is the dielectric breakdown strength.
- U_b is the measured breakdown voltage.
- d is the actual coating thickness at the relevant test location.
The dielectric breakdown behavior of ultrathin coatings may be influenced by pinholes, interfacial defects, electrode geometry, and local thickness variations.
Both breakdown voltage and calculated breakdown strength should therefore be recorded.
Dielectric breakdown testing is destructive. Specimens that have experienced breakdown should not subsequently be used as undamaged samples for other insulation reliability measurements.
(4) Partial Discharge Inception Voltage
Partial Discharge Inception Voltage (PDIV) is the applied voltage at which detectable partial discharge begins under specified measurement conditions.
A complete PDIV measurement procedure should define:
- Electrode geometry.
- Electrode contact conditions.
- Coating thickness.
- Applied voltage waveform.
- Ambient temperature.
- Relative humidity.
- Atmospheric pressure.
- Background electrical noise.
- Measurement sensitivity.
- Partial discharge detection criteria.
Where practical, internal coating discharge, interfacial discharge, and external air discharge originating from the test arrangement should be distinguished.
PDIV measurements during formulation screening are primarily intended to compare different dielectric coating systems under controlled conditions.
These measurements must not be directly interpreted as allowable operating voltages for actual busbar assemblies.
(5) Relative Permittivity and Dielectric Loss
Dielectric spectroscopy is used to investigate the influence of nanoparticle loading and solvent dilution on coating dielectric properties.
A preliminary frequency range of 100 Hz to 1 MHz may be considered, depending on equipment capabilities and application requirements.
The principal evaluation parameters include:
- Frequency-dependent relative permittivity.
- Frequency-dependent dielectric loss.
- Filler-related interfacial polarization.
- Dielectric stability at elevated temperatures.
- Changes in dielectric properties following damp-heat aging.
(6) Coating Adhesion
Cross-cut adhesion testing or appropriate pull-off adhesion testing may be used to evaluate coating-to-copper bonding performance.
For ultrathin coatings, the applicability of the selected adhesion test method must be evaluated according to coating thickness and substrate properties.
Failure morphology should also be documented.
Potential failure modes include:
- Cohesive failure within the coating.
- Adhesive failure at the copper-to-coating interface.
- Failure within the testing adhesive.
- Mixed-mode failure.
(7) Environmental Reliability
Preliminary environmental reliability screening should include damp-heat exposure and temperature cycling.
Table 11. Proposed Environmental Reliability Screening Conditions
| Test Item | Suggested Experimental Condition | Primary Evaluation Parameters |
|---|---|---|
| Steady-State Damp Heat | 85°C and 85% relative humidity | Insulation resistance, adhesion, appearance |
| Damp-Heat Exposure Duration | 168, 500, and 1,000 hours | Property retention |
| Thermal Cycling | -40°C to 125°C | Cracking, delamination, adhesion |
| Thermal Cycle Count | 100, 250, and 500 cycles | Coating integrity |
| High-Temperature Aging | According to material thermal endurance | Dielectric and thermal stability |
| Post-Aging Electrical Testing | Equivalent to initial test conditions | PDIV, breakdown strength, insulation resistance |
These conditions are proposed research parameters rather than universal qualification requirements for all busbar products.
Temperature transition rates, dwell times, recovery conditions, environmental exposure procedures, and failure criteria must be defined.
For coating materials unsuitable for the proposed temperature range, preliminary thermal stability evaluation should be conducted before selecting aging conditions.
2.4 Characterization During Flow Rate and Deposition Process Scale-Up
2.4.1 Testing Equipment
The primary objective of flow rate scale-up is to increase deposition capacity while maintaining coating morphology, thickness consistency, and electrical insulation reliability.
The original ultrasonic spray coating platform may be supplemented with:
- Precision liquid flow calibration equipment.
- Continuous liquid delivery and circulation systems.
- Spray pattern characterization equipment.
- High-speed imaging systems.
- Droplet size measurement equipment.
- Substrate temperature monitoring.
- Precision mass measurement equipment.
- Three-dimensional surface profilometry.
- Automated coating thickness measurement.
- Process data acquisition systems.
Where suitable equipment is available, laser diffraction or Phase Doppler Anemometry (PDA) may be used to characterize droplet size distributions under different liquid flow conditions.
Relevant droplet size parameters may include D10, D50, D90, and appropriate mean diameter values.
These measurements can help determine how formulation properties and liquid delivery rates influence ultrasonic atomization behavior.
2.4.2 Testing Items
(1) Liquid Flow Rate Stability
Actual liquid delivery should be calibrated by measuring the delivered mass or volume over a defined period.
Flow rate deviation can be calculated as:
Flow Deviation (%) = 100 x (Actual Flow Rate – Set Flow Rate) / Set Flow Rate
The investigation should include:
- Continuous liquid delivery stability.
- Short-term flow fluctuations.
- Start-stop repeatability.
- Long-duration operating stability.
- Changes associated with ink viscosity.
- Filler sedimentation effects.
(2) Spray Pattern and Single-Track Deposition Morphology
Single-track coating experiments should be conducted to characterize the effective spray pattern.
The principal evaluation parameters include:
- Effective spray width.
- Single-track deposition thickness.
- Transverse thickness distribution.
- Center-to-edge deposition differences.
- Droplet deposition distribution.
- Localized liquid accumulation.
Single-track deposition results provide a basis for determining appropriate raster path spacing and spray pattern overlap.
(3) Material Transfer Efficiency
Effective solids deposition efficiency can be estimated from actual dielectric ink consumption and the retained dry coating mass.
The calculation is expressed as:
Transfer Efficiency (%) = 100 x M_deposited / M_supplied_solids
Where:
- M_deposited is the net mass of the cured coating retained on the copper substrate.
- M_supplied_solids is the nonvolatile solid mass contained in the supplied dielectric ink.
Liquid retained in delivery lines, nozzle priming losses, cleaning losses, and overspray outside the effective coating region should be documented separately.
This distinction is important when comparing laboratory deposition efficiency with overall industrial material utilization.
(4) Coating Thickness Uniformity
Multipoint thickness measurements are used to characterize coatings prepared at different liquid flow rates and scanning speeds.
Thickness uniformity can be evaluated using the coefficient of variation:
CV (%) = 100 x SD / T_avg
Where:
- CV is the coating thickness coefficient of variation.
- SD is the standard deviation of the measured coating thickness.
- T_avg is the average measured coating thickness.
A lower coefficient of variation generally indicates lower relative thickness variation within the measured area.
However, minimum local coating thickness must also be evaluated.
Average coating thickness alone may conceal electrically critical thin regions.
(5) Deposition Rate
Deposition efficiency can be evaluated through the relationship between actual retained coating mass or coating thickness and effective spraying duration.
Particular attention should be paid to whether increasing liquid flow rate while proportionally increasing scanning speed can maintain comparable material deposition per unit area.
The objective is to establish whether improved process throughput can be achieved without compromising coating integrity.
(6) Electrical Performance Reassessment
Samples manufactured using different liquid flow rates and scanning speeds should undergo insulation resistance, dielectric breakdown, and PDIV testing.
Two complementary comparison methods are recommended.
The first method compares coatings prepared using the same number of deposition passes.
This approach evaluates the influence of process parameters on actual thickness growth and deposition efficiency.
The second method compares coatings with approximately equivalent final dry-film thicknesses.
This approach evaluates the effects of atomization behavior and film formation conditions while reducing interference caused by thickness differences.
2.5 Characterization of 100 cm2 Scale-Up Specimens
2.5.1 Testing Equipment
Characterization of 100 cm2 specimens requires additional spatial distribution measurements and large-area defect evaluation.
The proposed testing platform may include:
- Automated XY thickness measurement platform.
- Eddy-current coating thickness measurement equipment.
- Three-dimensional optical profilometry.
- High-resolution industrial machine vision.
- Suitable coating pinhole detection equipment.
- Large-area and localized test electrodes.
- Partial discharge measurement equipment.
- High-voltage insulation testing systems.
- Environmental reliability chambers.
The evaluation should emphasize spatial variations in coating properties rather than relying exclusively on overall average values.
2.5.2 Testing Items
(1) Twenty-Five-Point Coating Thickness Distribution
The 100 mm x 100 mm substrate is divided into five rows and five columns.
Measurement locations are positioned at 10, 30, 50, 70, and 90 mm along both principal axes, establishing a 25-point thickness measurement matrix.
Table 12. Thickness Measurement Matrix for 100 cm2 Specimens
| Y/X Coordinate | 10 mm | 30 mm | 50 mm | 70 mm | 90 mm |
|---|---|---|---|---|---|
| 10 mm | To be measured | To be measured | To be measured | To be measured | To be measured |
| 30 mm | To be measured | To be measured | To be measured | To be measured | To be measured |
| 50 mm | To be measured | To be measured | To be measured | To be measured | To be measured |
| 70 mm | To be measured | To be measured | To be measured | To be measured | To be measured |
| 90 mm | To be measured | To be measured | To be measured | To be measured | To be measured |
Additional measurements should be performed closer to the substrate edges, including appropriate cross-sectional measurements.
The planar 25-point measurement matrix does not fully characterize coating coverage on vertical sidewalls, sharp edges, or rounded conductor corners.
The principal statistical parameters include:
- Average coating thickness.
- Maximum coating thickness.
- Minimum coating thickness.
- Thickness standard deviation.
- Thickness coefficient of variation.
- Edge-to-center thickness ratio.
(2) Large-Area Pinhole and Defect Detection
Automated optical inspection and validated electrical coating discontinuity detection methods may be used to characterize defects across the 100 cm2 coating area.
Pinhole density can be calculated as:
Pinhole Density = Number of Detected Pinholes / Coated Area
The result may be expressed as defects per cm2.
For electrically critical regions, acceptance criteria for through-thickness pinholes must be established according to the insulation design requirements.
The absence of detected pinholes does not establish the absence of defects below the detection limit of the selected inspection method.
(3) Electrical Performance at Different Specimen Locations
Electrical testing regions may be established at the specimen center, corners, and near-edge locations.
The principal evaluation items include:
- Dielectric breakdown performance at central regions.
- Electrical insulation performance near edges.
- Insulation resistance at different locations.
- PDIV under defined electrode configurations.
- Correlation between electrical failure locations and coating defects.
Destructive electrical test locations should be sufficiently separated.
Alternatively, independently prepared scale-up specimens should be used to prevent previous breakdown damage from influencing subsequent measurements.
(4) Adhesion of Scale-Up Specimens
Coating adhesion should be evaluated at selected central, edge, and different scanning regions.
This investigation determines whether changes in spray trajectories and local drying conditions influence interfacial bonding performance.
(5) Performance Consistency After Environmental Aging
Selected damp-heat and thermal cycling conditions should be applied to 100 cm2 specimens.
The following properties should be compared before and after environmental exposure:
- Coating appearance.
- Surface roughness.
- Adhesion.
- Insulation resistance.
- PDIV.
- Dielectric breakdown strength.
- Crack formation.
- Interfacial defect development.
These measurements provide a basis for determining whether small-area ultrasonic spray coating processes can be transferred to larger busbar-related substrates while maintaining acceptable coating consistency.
3. Results and Discussion
This section establishes the proposed analytical framework and discusses the physical mechanisms expected to influence coating performance.
Actual experimental measurements have not yet been provided.
The following discussions therefore represent theoretical interpretations and testable research hypotheses rather than completed experimental findings.
3.1 Influence of Dielectric Ink Composition
Dielectric ink formulation determines ultrasonic atomization behavior, droplet deposition, solvent evaporation, nanoparticle distribution, and the resulting polymer coating microstructure.
Variations in I-NP and S-NP ratios may influence insulation coating performance through different mechanisms.
The I-NP ratio primarily affects the continuous polymer phase, nanoparticle interfaces, filler loading, and cured coating microstructure.
The S-NP ratio primarily affects ink rheology, atomization stability, wet-film formation, and solvent evaporation behavior.
These variables should initially be investigated separately and subsequently optimized together.
3.1.1 Analysis of the Insulating Matrix-to-Nanoparticle Ratio (I-NP)
In this study, I-NP refers to the mass ratio between the electrically insulating polymer matrix and nanoparticles.
It does not refer to an ion-conducting polymer or ionomer matrix.
Busbar dielectric coatings require high electrical resistance, and formulation principles developed for ion-conducting electrochemical membranes cannot be directly transferred to electrical insulation applications.
(1) Influence of I-NP Ratio on Ink Viscosity
Increasing nano-Al2O3 content increases particle concentration and may intensify interparticle interactions.
Due to their relatively high specific surface area, nanoparticles may adsorb polymer molecules and dispersants, affecting polymer chain mobility and suspension rheology.
At relatively low filler loading, particle separation is generally greater, potentially allowing the dielectric ink to maintain favorable flow characteristics.
As nanoparticle loading increases, interparticle interactions and agglomeration may become more significant.
This behavior can increase apparent viscosity and introduce non-Newtonian flow characteristics.
High-viscosity dielectric inks may result in:
- Unstable liquid distribution across the ultrasonic atomizing surface.
- Irregular atomization.
- Changes in droplet size distribution.
- Reduced spray pattern consistency.
- Increased liquid delivery resistance.
- Material accumulation on the nozzle.
- Increased blockage risk.
Consequently, an appropriate I-NP ratio must satisfy both functional material requirements and ultrasonic spray coating process compatibility.
(2) Influence of I-NP Ratio on Coating Microstructure
At relatively low filler loading, epoxy resin forms the primary continuous insulating phase, with nanoparticles dispersed throughout the polymer matrix.
Under suitable dispersion and interfacial bonding conditions, nanoparticles may modify local microstructure and polymer-filler interactions.
However, excessive nanoparticle loading or insufficient dispersion may produce heterogeneous agglomerated regions.
Such regions may exhibit:
- Incomplete resin wetting.
- Interfacial micropores.
- Localized curing shrinkage differences.
- Nonuniform filler concentration.
- Reduced polymer phase continuity.
Cross-sectional SEM characterization should therefore determine whether each I-NP formulation produces a sufficiently continuous and dense insulating polymer structure.
(3) Influence of I-NP Ratio on Dielectric Breakdown Performance
The introduction of nanoparticles increases the number of internal polymer-filler interfaces.
These interfaces may influence charge carrier transport, polarization behavior, and localized electric field distribution.
Appropriate nanoparticle dispersion and interfacial bonding may suppress certain charge transport mechanisms or reduce selected structural defects.
Conversely, nanoparticle agglomeration, microscopic voids, or dielectric permittivity differences may generate localized electric field enhancement.
Such effects can reduce dielectric breakdown strength.
The relationship between nanoparticle loading and dielectric breakdown strength may therefore be nonmonotonic.
Depending on the selected resin, nanoparticle surface treatment, and processing conditions, dielectric breakdown strength may increase, decrease, or exhibit an intermediate optimum.
The actual relationship must be established experimentally.
Dielectric breakdown results should be correlated with:
- Actual dry-film thickness.
- Nanoparticle loading.
- Surface roughness.
- Coating porosity.
- Particle agglomeration.
- Interfacial bonding.
- Curing conditions.
(4) Influence of I-NP Ratio on Partial Discharge Inception Voltage
Nanoparticles may influence partial discharge behavior by modifying dielectric permittivity, interfacial structure, and charge transport mechanisms.
Well-dispersed nanocomposite coatings may offer opportunities to improve interfacial defect control and resistance to electrical degradation.
However, increasing nanoparticle loading does not necessarily increase PDIV.
If microscopic voids or debonded regions develop around agglomerated particles, electric field redistribution between solid dielectric materials and gas-filled defects may promote partial discharge inception.
PDIV measurements should therefore be interpreted together with coating morphology, electrode configuration, local thickness, and discharge source identification.
Nanoparticle loading alone is insufficient to explain the partial discharge characteristics of a complete insulation structure.
(5) Comprehensive Evaluation of I-NP Formulations
Different nanoparticle loading levels may exhibit the technical characteristics summarized in Table 13.
Table 13. Potential Influence of Different I-NP Ratios
| Filler Loading Level | Potential Advantages | Potential Risks |
|---|---|---|
| Unfilled Epoxy | Continuous polymer phase and simple formulation | Limited functional modification |
| Low Filler Loading | Favorable dispersion and sprayability | Limited contribution from functional fillers |
| Intermediate Filler Loading | Potential balance between dielectric and interfacial properties | Requires dispersion and wettability optimization |
| High Filler Loading | Greater functional filler content | Increased viscosity, agglomeration, and defect risks |
Selection of the preferred formulation should be based on comprehensive performance evaluation rather than maximizing nanoparticle loading or dielectric breakdown strength alone.
3.1.2 Analysis of the Solvent-to-Nanoparticle Dilution Ratio (S-NP)
The S-NP ratio is an important parameter governing dielectric ink sprayability.
Adjusting solvent concentration modifies ink solids content, viscosity, surface tension, and evaporation behavior.
These characteristics directly influence ultrasonic atomization, droplet deposition, and coating formation.
(1) Low S-NP Ratio Formulations
A relatively low solvent concentration generally results in higher solids content.
Potential advantages include greater solid material deposition during each coating pass and increased dry-film thickness growth.
However, high-solids formulations may exhibit:
- Increased viscosity.
- Reduced atomization stability.
- Insufficient droplet spreading.
- Increased particle interactions.
- Greater agglomeration risk.
- Increased liquid delivery resistance.
- Material accumulation within the coating system.
The maximum practical solids content must therefore be established through formulation-specific and nozzle-specific testing.
(2) High S-NP Ratio Formulations
Increasing solvent concentration may reduce ink viscosity and improve the ultrasonic sprayability of certain relatively viscous formulations.
However, excessive dilution reduces the quantity of effective solid material contained within a given liquid volume.
Under equivalent liquid flow rate and scanning conditions, dry-film thickness per deposition pass decreases as the volume solids fraction decreases.
Additional disadvantages of excessive solvent dilution may include:
- Increased number of deposition passes.
- Increased overall solvent consumption.
- Longer drying requirements.
- Localized liquid accumulation.
- Drying-induced shrinkage.
- Potential redistribution of functional fillers.
- Increased VOC emissions.
The highest achievable dilution ratio should not automatically be considered the optimum coating formulation.
(3) Solvent Evaporation and Droplet Film Formation
During ultrasonic spray coating, droplets undergo several physical stages:
Atomization → Droplet Transport → Substrate Impact → Droplet Spreading → Solvent Evaporation → Polymer Film Formation → Curing.
If the solvent evaporation rate is excessively high, droplets may become concentrated before reaching the substrate or during spreading.
This behavior may result in particle accumulation, increased surface roughness, and insufficient coalescence between neighboring droplets.
If solvent evaporation is excessively slow, droplets may remain mobile on the substrate for extended periods.
Under high liquid deposition conditions, this may lead to sagging, localized pooling, filler redistribution, and thickness variation.
Consequently, solvent system optimization must consider not only ink viscosity but also:
- Solvent evaporation rate.
- Surface tension.
- Copper substrate wettability.
- Polymer compatibility.
- Nanoparticle dispersion.
- Substrate temperature.
- Final curing behavior.
(4) Coffee-Ring Effect
During the drying of certain particle-containing droplets, differences in evaporation rate and internal liquid flow may transport suspended particles toward the droplet perimeter.
This phenomenon is commonly known as the coffee-ring effect.
For busbar insulation coatings, pronounced nanoparticle redistribution may cause localized filler enrichment, increased surface roughness, and heterogeneous dielectric microstructures.
Potential control approaches include optimization of:
- Solvent composition.
- Substrate temperature.
- Droplet deposition density.
- Ink rheology.
- Surface wettability.
- Multiple thin-film deposition passes.
- Intermediate drying conditions.
The effectiveness of these approaches must be investigated for the specific dielectric ink formulation.
(5) Principles for S-NP Ratio Optimization
An appropriate S-NP ratio should balance:
- Ultrasonic atomization stability.
- Nanoparticle dispersion stability.
- Droplet spreading.
- Coating density.
- Dry-film deposition efficiency.
- Residual solvent control.
- Electrical insulation performance.
- Manufacturing cycle time.
- Material consumption.
- Environmental requirements.
The optimum dielectric ink formulation is not necessarily the formulation exhibiting the lowest viscosity or the highest solvent content.
3.2 Analysis of Deposition Process Parameters
3.2.1 Influence of Liquid Flow Rate on Coating Formation
Liquid flow rate is one of the principal parameters governing ultrasonic spray coating deposition efficiency.
At constant scanning speed and path spacing, increasing liquid flow rate increases theoretical material delivery per unit area.
However, actual dry-film thickness growth also depends on atomization capacity, effective material transfer efficiency, droplet deposition behavior, and film formation.
At relatively low liquid flow rates, deposited droplets may have sufficient time to spread and release solvent.
This may facilitate precise thin-film thickness control.
Nevertheless, insufficient droplet coverage may result in discontinuous film formation or excessive drying between droplets.
At higher liquid flow rates, wet-film formation becomes more rapid, potentially improving deposition efficiency.
If the flow rate exceeds the stable atomization window of the selected ultrasonic nozzle, larger droplets, unstable liquid films, localized accumulation, and increased thickness variation may occur.
Consequently, the maximum practical liquid flow rate should be determined by coating quality and atomization stability rather than equipment flow capacity alone.
3.2.2 Influence of Scanning Speed on Coating Uniformity
Nozzle scanning speed directly influences material deposition per unit scanning length.
A relatively low scanning speed generally results in greater liquid deposition per unit area.
However, excessive deposition may increase wet-film movement, sagging, and localized pooling.
Higher scanning speeds can reduce deposition thickness per pass and potentially improve manufacturing throughput.
If scanning speed becomes excessively high relative to the liquid flow rate, insufficient material deposition may produce incomplete coating coverage or discontinuous films.
Appropriate scanning speed must therefore be selected together with spray pattern width, path spacing, and required coating thickness.
3.2.3 Coordinated Scale-Up of Liquid Flow Rate and Scanning Speed
Under ideal conditions, with other parameters maintained constant, the ratio between liquid flow rate and scanning speed provides a useful reference for material delivery per unit scanning length.
The following experimental combinations are proposed.
Table 14. Process Combinations with Equivalent Theoretical Material Delivery
| Process Combination | Liquid Flow Rate | Scanning Speed | Relative Material Delivery |
|---|---|---|---|
| P-1 | 0.2 mL/min | 25 mm/s | 1.0 |
| P-2 | 0.4 mL/min | 50 mm/s | 1.0 |
| P-3 | 0.6 mL/min | 75 mm/s | 1.0 |
| P-4 | 0.8 mL/min | 100 mm/s | 1.0 |
These four combinations have equivalent theoretical liquid delivery per unit scanning length.
If spray pattern geometry, path spacing, solids content, and effective transfer efficiency remain unchanged, their theoretical average dry-film thicknesses should be similar.
However, increasing liquid flow rate may modify the liquid film on the ultrasonic nozzle surface, droplet size distribution, and actual deposition efficiency.
Equivalent flow-to-speed ratios therefore do not guarantee identical coating microstructure, surface roughness, or electrical insulation performance.
The principal objective of this investigation is to determine whether manufacturing throughput can be increased through coordinated adjustment of liquid flow rate and scanning speed without compromising coating quality.
3.2.4 Relationship Between Theoretical and Actual Coating Thickness
Assuming a volume solids content of 15%, effective deposition efficiency of 80%, and scanning path spacing of 3 mm, theoretical average dry-film thicknesses can be calculated for different flow rate and scanning speed combinations.
Table 15. Theoretical Dry-Film Thickness per Complete Area Scan
Unit: microns per pass.
| Liquid Flow Rate | 25 mm/s | 50 mm/s | 100 mm/s |
|---|---|---|---|
| 0.2 mL/min | 5.33 | 2.67 | 1.33 |
| 0.4 mL/min | 10.67 | 5.33 | 2.67 |
| 0.6 mL/min | 16.00 | 8.00 | 4.00 |
| 0.8 mL/min | 21.33 | 10.67 | 5.33 |
These values are theoretical predictions rather than measured coating thicknesses.
Actual dry-film measurements should be compared with theoretical estimates to identify process-specific deviations.
Potential sources of deviation include:
- Droplet overspray.
- Changes in effective spray width.
- Droplet rebound or material loss.
- Variations in ink solids content.
- Nanoparticle sedimentation.
- Motion platform acceleration and deceleration.
- Additional curing shrinkage.
- Differences in copper substrate wettability.
- Variations in atomization behavior.
A calibrated deposition model can subsequently be established to improve process parameter selection and coating thickness prediction.
3.2.5 Comparison of Multiple Thin-Film Passes and Fewer Thick-Film Passes
At approximately equivalent final dry-film thickness, different deposition strategies may be compared to investigate the influence of individual pass thickness on coating quality.
A target dry-film thickness of 30 microns is selected as an illustrative experimental condition.
Table 16. Comparison of Multiple-Pass Deposition Strategies
| Deposition Strategy | Target Average Thickness per Pass | Theoretical Complete Scanning Passes |
|---|---|---|
| A | 3 microns | 10 |
| B | 5 microns | 6 |
| C | 10 microns | 3 |
| D | 15 microns | 2 |
Multiple thin-film deposition passes may facilitate:
- Precise thickness adjustment.
- Improved control of wet-film deposition.
- Solvent release between passes.
- Reduced localized liquid accumulation.
- Localized coating reinforcement.
- Multilayer functional coating design.
However, increasing the number of passes may extend manufacturing cycle time and introduce interlayer adhesion concerns.
Fewer thick-film passes may improve deposition throughput.
Nevertheless, thicker wet-film deposition places greater demands on solvent evaporation, leveling, bubble release, and curing stress management.
The appropriate deposition strategy must balance coating integrity, electrical insulation performance, and manufacturing efficiency.
3.2.6 Comprehensive Deposition Process Optimization
The following response variables are recommended for ultrasonic spray coating process optimization:
- Average dry-film thickness.
- Minimum local dry-film thickness.
- Thickness coefficient of variation.
- Surface roughness.
- Pinhole density.
- Effective material transfer efficiency.
- Dielectric breakdown strength.
- Partial Discharge Inception Voltage.
- Effective spraying duration.
- Manufacturing cycle time.
- Adhesion.
- Electrical performance retention after environmental aging.
Analysis of Variance (ANOVA) may be used to investigate the principal effects of process parameters.
Where sufficient experimental data are available, Response Surface Methodology (RSM) may be employed to establish quantitative relationships between deposition parameters and coating performance.
The optimization process should first satisfy electrical insulation and coating integrity requirements.
Material utilization and manufacturing throughput should subsequently be optimized within the validated quality window.
3.3 Scale-Up to 100 cm2 Specimens
3.3.1 Deposition Uniformity During Area Scale-Up
Increasing the coating area from 25 cm2 to 100 cm2 may influence actual coating uniformity even when theoretical deposition per unit area remains unchanged.
Potential contributing factors include:
- Increased scanning path length.
- Extended continuous nozzle operating time.
- Time-dependent changes in ink viscosity.
- Nanoparticle sedimentation.
- Spatial variations in substrate temperature.
- Different drying conditions between early and late deposited regions.
- Nozzle start-stop behavior.
- Scanning direction changes.
- Motion platform acceleration and deceleration.
Process scale-up should therefore not be considered simply an increase in spraying duration.
It represents a coordinated evaluation of liquid delivery stability, motion control, solvent evaporation, coating morphology, and manufacturing consistency.
3.3.2 Comparison of Unidirectional and Crosshatch Scanning
Unidirectional raster scanning offers relatively simple programming and straightforward trajectory planning.
However, nonuniform overlap between adjacent spray patterns may generate periodic thickness variations along a preferred direction.
Crosshatch scanning alternates the scanning direction between successive deposition cycles.
This approach may reduce the accumulation of directional coating streaks and improve spatial thickness uniformity.
Nevertheless, crosshatch scanning may also change:
- Intermediate drying duration.
- Droplet overlap.
- Wet-film spreading.
- Layer-to-layer deposition behavior.
- Overall manufacturing cycle time.
The actual advantages of each scanning strategy should be evaluated using 25-point thickness measurements, three-dimensional surface morphology, and electrical performance testing.
3.3.3 Edge Compensation Mechanisms
Copper substrate edges and actual busbar rounded corners represent electrically critical coating regions.
During spraying, edge regions may exhibit reduced coating thickness due to spray pattern truncation, insufficient droplet deposition, localized wetting differences, or liquid redistribution.
At the same time, conductor edges may produce localized electric field concentration.
The combination of reduced coating thickness and increased electric field strength can create electrically vulnerable regions.
Potential edge compensation methods include:
- Optimization of scanning start and end positions.
- Adjustment of nozzle orientation.
- Additional localized scanning passes.
- Region-specific scanning speed control.
- Multi-axis workpiece positioning.
- Controlled workpiece rotation.
- Optimization of actual conductor corner radius.
For 100 cm2 planar specimens, edge compensation primarily evaluates two-dimensional surface coating uniformity.
Actual busbar sidewalls, rounded corners, mounting holes, and bending regions require dedicated three-dimensional coating validation.
3.3.4 Quality Evaluation of Scale-Up Specimens
The following evaluation framework is proposed to compare small-area specimens and 100 cm2 scale-up specimens.
Table 17. Performance Comparison Framework for Area Scale-Up
| Evaluation Parameter | 25 cm2 Specimens | 100 cm2 Specimens |
|---|---|---|
| Average Dry-Film Thickness | To be measured | To be measured |
| Minimum Dry-Film Thickness | To be measured | To be measured |
| Thickness Standard Deviation | To be measured | To be measured |
| Thickness Coefficient of Variation | To be measured | To be measured |
| Surface Roughness | To be measured | To be measured |
| Pinhole Density | To be measured | To be measured |
| Dielectric Breakdown Strength | To be measured | To be measured |
| PDIV | To be measured | To be measured |
| Adhesion | To be measured | To be measured |
| Material Transfer Efficiency | To be measured | To be measured |
| Processing Time per Unit Area | To be measured | To be measured |
| Electrical Performance After Damp-Heat Aging | To be measured | To be measured |
Average thickness deviation, thickness coefficient of variation, and minimum local thickness may be selected as preliminary process scale-up control parameters.
For example, the following candidate process development targets may be considered:
- Average thickness deviation within 10% of the specified target.
- Thickness coefficient of variation not exceeding 5%.
These values are illustrative internal research targets.
They are not established industry-wide acceptance criteria for busbar insulation coatings.
Actual acceptance limits must be determined according to measurement capability, insulation design, operating voltage, environmental conditions, and applicable product safety requirements.
3.3.5 Electrical Performance and Area Effects
Large-area dielectric coatings may exhibit different statistical electrical breakdown behavior compared with small-area specimens.
As the electrically stressed area increases, the probability of including a critical microscopic defect may also increase.
Relevant defects include:
- Through-thickness pinholes.
- Nanoparticle agglomerates.
- Interfacial voids.
- Localized thin coating regions.
- Microscopic cracks.
- Contamination.
Consequently, specimens with equivalent average coating thickness and identical material formulations may still exhibit different dielectric breakdown distributions when tested using different effective electrode areas.
Weibull statistical analysis may be employed to investigate dielectric breakdown behavior.
The two-parameter Weibull cumulative distribution function can be expressed in plain text as:
F(E) = 1 – exp[-(E / alpha)^beta]
Where:
- F(E) is the cumulative probability of dielectric breakdown.
- E is the dielectric breakdown field strength.
- alpha is the characteristic dielectric breakdown field strength.
- beta is the Weibull shape parameter.
- exp represents the exponential function.
The characteristic breakdown field strength represents the field corresponding to approximately 63.2% cumulative breakdown probability in the two-parameter Weibull model.
The Weibull shape parameter provides information regarding the statistical dispersion of breakdown results.
Comparing characteristic breakdown strength and statistical dispersion under different effective electrical test areas can support investigation of area-dependent insulation reliability.
It is essential to distinguish the total coated surface area from the effective electrically stressed electrode area.
Increasing the coated specimen area alone does not necessarily increase the electrical test area.
Statistically meaningful area-effect models require sufficient independent breakdown measurements, consistent test conditions, and appropriately defined electrode configurations.
3.3.6 Extension from 100 cm2 Specimens to Actual Busbar Manufacturing
Following completion of the 100 cm2 planar scale-up investigation, the ultrasonic spray coating process should be extended to representative busbar geometries.
Recommended research objects include:
- Straight copper busbars.
- Busbars with 90-degree bends.
- Busbars containing electrical connection holes.
- Busbars with different corner radii.
- Irregular high-voltage busbars.
- Laminated busbars.
- SiC power module interconnection busbars.
The experimental focus should progressively extend from planar coating uniformity toward three-dimensional manufacturing requirements.
Important investigation areas include:
- Three-dimensional coating coverage.
- Minimum insulation thickness around conductor edges.
- Masking accuracy at electrical connection regions.
- Programmable spray trajectories for complex geometries.
- Multi-axis automated motion control.
- PDIV measurements using representative busbar assemblies.
- Thermal cycling and mechanical vibration reliability.
- Continuous automated coating consistency.
- Production throughput and material utilization.
- Long-term coating quality traceability.
Scale-up to 100 cm2 primarily represents an intermediate laboratory-scale demonstration of area expansion.
It does not establish industrial mass-production readiness.
Further investigations involving larger substrates, multiple consecutive workpieces, complex three-dimensional busbars, extended equipment operation, and actual manufacturing cycle times are required.
4. Conclusions
This study establishes an experimental research framework for the preparation of ultrathin and uniform busbar insulation coatings using ultrasonic precision spray coating.
The proposed methodology covers dielectric ink formulation screening, deposition parameter optimization, morphological characterization, electrical performance evaluation, environmental reliability testing, and scale-up to 100 cm2 substrates.
Based on the proposed experimental design and theoretical coating formation mechanisms, the following research conclusions and hypotheses can be established.
Conclusion 1: Dielectric Ink Composition Is Fundamental to Ultrasonic Spray Coating Performance
The insulating matrix-to-nanoparticle ratio (I-NP) primarily influences ink rheological behavior, nanoparticle dispersion, polymer phase continuity, interfacial structure, and dielectric properties.
The solvent-to-nanoparticle ratio (S-NP) primarily influences ink dilution, ultrasonic atomization, droplet spreading, solvent evaporation, and dry-film formation.
These formulation parameters must be optimized together to establish an appropriate balance between sprayability and electrical insulation performance.
Conclusion 2: Liquid Flow Rate and Scanning Speed Govern Material Deposition per Unit Area
Under ideal steady-state deposition conditions, average coating thickness is positively related to liquid flow rate, volume solids content, effective deposition efficiency, and the number of complete deposition passes.
Coating thickness is inversely related to scanning speed and scanning path spacing.
Theoretical deposition models, combined with experimental calibration, can provide quantitative guidance for precision dry-film thickness control.
Conclusion 3: Coordinated Flow Rate and Scanning Speed Scale-Up Offers Potential Manufacturing Advantages
Increasing liquid flow rate while proportionally increasing scanning speed may improve production throughput while maintaining approximately equivalent theoretical material deposition per unit area.
However, increased liquid flow may influence ultrasonic atomization behavior, droplet size distribution, effective spray width, and actual material transfer efficiency.
The achievable process scale-up window must therefore be determined through experimental morphology and electrical insulation evaluation.
Conclusion 4: Multiple Thin-Film Deposition Passes Provide a Flexible Coating Thickness Control Method
Controlling individual deposition thickness, scanning cycles, and intermediate drying conditions provides opportunities to fabricate insulation coatings with different total thicknesses and multilayer structures.
This approach may be particularly useful for:
- Precision insulation coating.
- Localized edge reinforcement.
- Complex busbar geometries.
- Region-specific thickness control.
- Functional multilayer coating development.
Conclusion 5: Scale-Up to 100 cm2 Provides an Intermediate Step Toward Industrial Busbar Manufacturing
Comparing unidirectional raster scanning, crosshatch scanning, and localized edge compensation can provide insights into coating uniformity during area scale-up.
Combined with multipoint thickness measurements, pinhole detection, adhesion testing, and electrical performance evaluation, these investigations establish a framework for assessing larger-area coating consistency.
Conclusion 6: Ultrathin Coating Development Must Remain Consistent with Electrical Safety Requirements
Reduced average coating thickness and improved thickness uniformity do not independently establish suitability for high-voltage busbar insulation.
Electrical reliability must be evaluated through a comprehensive assessment of:
- Minimum local insulation thickness.
- Dielectric breakdown strength.
- Partial Discharge Inception Voltage.
- Interfacial adhesion.
- Environmental aging.
- Actual busbar geometry.
- Maximum operating voltage.
- Applicable electrical safety requirements.
Overall, ultrasonic precision spray coating represents a promising manufacturing technology for investigating ultrathin insulation coatings, localized protection of complex busbar geometries, and multilayer functional material deposition.
Future research should focus on:
- High-solids dielectric ink formulations.
- Stable high-flow ultrasonic atomization.
- Multi-nozzle coordinated deposition.
- Three-dimensional busbar precision coating.
- Inline coating thickness inspection.
- Automated defect detection.
- High-frequency repetitive impulse partial discharge.
- Long-term electrothermal aging.
- Industrial manufacturing process scale-up.
By establishing coordinated relationships among insulation material formulation, ultrasonic atomization equipment, precision deposition processes, coating microstructure, and electrical reliability, ultrasonic spray coating may provide a flexible and experimentally verifiable manufacturing solution for advanced busbars used in electric vehicles, energy storage systems, and SiC-based high-frequency power electronics.
Research Statement and Technical Disclaimer
This article presents a proposed experimental methodology and technical analysis framework for ultrasonic spray coating of busbar insulation materials.
The dielectric ink formulations, nanoparticle loading ratios, liquid flow rates, scanning speeds, coating thicknesses, deposition efficiencies, scale-up parameters, and environmental reliability conditions are proposed research parameters or theoretical calculations.
They do not represent independently verified experimental results, established optimum formulations, guaranteed equipment capabilities, or qualified product performance specifications.
Actual optimum dielectric ink compositions, dielectric breakdown strength, Partial Discharge Inception Voltage, coating adhesion, material transfer efficiency, and long-term environmental reliability must be determined through experimental measurements.
All high-voltage busbar insulation applications require application-specific engineering qualification and compliance with relevant electrical safety requirements.
The referenced publications and technical standards should be checked for bibliographic accuracy, current editions, and applicability before formal academic or commercial publication.